Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

fuel gas pipes flushing

Status
Not open for further replies.

pekos

Mechanical
Joined
Mar 15, 2005
Messages
12
Location
MA
We have troubles with our furnaces fuel gas system, frequent clogging problems in burners and their feeding piping branches..so we are considering a flushing of the pipes
we used to do it with steam (3-4 bar), but got no results.
is there any means to use a more efficient solution to flush these pipes?
 
What's causing the plugging?
 
TD2K
I did some analysis on deposits sample:
Iron: 24.4%
Manganese: 0.14%
lead: 0.15%
zn: .04%
antimony: 0.07%
Cu: 0.02%

loss at 550°c: 22%
 