Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Frozen pipe - pressure exerted on pipe

Status
Not open for further replies.

vesselguy

Petroleum
Joined
Feb 25, 2002
Messages
386
Location
CA
Morning,
I have heard that a segment of piping in one of our plant was frozen with the hydrotest water in it. Although it is not related to my area of responsibility, I was thinking how I could calculate the pressure exerted by the expanded water in the solid phase. It's been a long time since 1st year university and I don't even have my 3-phases of matter book anymore. Can anyone point me to a source that can show me how I can calculate the pressure excerted by the ice on the pipe? Meanwhile, I'd try to search the web and when I get home, I'd search my Mark's handbook.

Thanks.
 
Wow, during my net search, I found out there are 10 kinds of ice and a guy can actually have job studying ice!
It's coming back a little at a time now.. I think the pressure is calculated by using constant volumn equation in thermodynamics, which as I recall (poorly at that), is

Work (1-2) = V x delta P.

 
Question: were the ends of the pipe blocked off while the pipe was frozen?

Other than that, not that I know a lot in this area, it must not be too big a deal, or companies wouldn't be able to use freeze seals to isolate water lines for maintenance.

Patricia Lougheed

Please see FAQ731-376 for tips on how to make the best use of the Eng-Tips Forums.
 
Determine if pipe is restrained longitudinally.
Determine if pipe was open to atmosphere or sealed off as it froze (ie, some of the expansion takes place before the water freezes).
Calculate mass of water in a unit length of pipe.
Calculate equivalent volume of ice this represents.
Find bulk modulus of ice.
Assume different pressures. Calculate reduction in ice volume due to the pressure, and increase in pipe volume due to the pressure until you get a match- considering longitudinal expansion also if not restrained.
First pressure to guess would be the one corresponding to yield point of pipe. If the final answer is above this pressure, you probably won't have a good idea of how the pipe behaved.

I can see how a line might start freezing at one point, and build up more and more pressure as it froze down the line, if it was closed off at the far end.
 
I don't know if you can calculate an open ended pipe or not, I just remember the experiment where they place a 3 in diameter ball wthat had a 1" diameter void in it filled with water. The ball split apart when placed in a freezer.

On a practicle note, I was replacing some pipe and making tie ins in a gas plant located in a climate that can freeze. One of the lines I decided to replace was a 8" bypass around a TEG contactor. The line droped down and went undergroud around the tower and went up and reconnected to the tower outlet. At the tower outlet side was a block valve that was the by-pass valve.

When we dug up the buried line, the paint and coating were split along the longitude of the pipe. When we mesured the OD, the pipe was bigger than 8 5/8", closer 8 3/4. The buried dead leg accumulated water and froze over the 20 years it was in service.
 
I did this analysis a few decades ago, looking at using a freeze plug to isolate for a new tee. As I recall, the start of the freeze had some ability to move laterally (the line was water-full and vented) and pressure was pretty constant. Increasing the length of either of the freeze plugs toward the other one quickly used up that small movement. Once the plugs were fixed in place (by the length of the freeze) then any additional freezing on the trapped side resulted in amazingly high pressures very rapidly. The numbers I recall were on the order of dozens of bar per gram of additional ice.

David
 