Does anyone call up specific surface preparation for friction grip bolts on their drawings or specifications. I have a galvanized member which I have called up friction grip bolts. I noticed the steelwork shop drawings makes comment that painted surfaces are not allowed around friction grip bolts but doesn't say anything about galvanized steel.
I was reading through an industrial galvanizers association website which says that the galvanized surface should be roughed by grinding or sand-blasting.
Does anyone actually specify this.
I was reading through an industrial galvanizers association website which says that the galvanized surface should be roughed by grinding or sand-blasting.