MetalHead83
Materials
As the header suggests, I'm looking for some literature for my research/investigation that can help differentiate the appearance of debris from a Deflagration vs Detonation perspective.
There are many aspects of the investigation I cannot talk about based on contracts/ legal constraints, so I posed the Question as general one about literature for my research/ investigation. I am currently digging through the AMS Hbk 12 on Fractography.
Background:
I'm a materials engineer with a fair bit of experience in failure analysis and fractography (abt 15 yrs)
The Ordnance was known and intended, a portion of the housing system failed in a closed-system.
I believe I have narrowed down the origin point of the housing failure as a whole (eliminating origin features on other debris items as secondary)
The event was so quick (1-2 ms) the pressure transducer data collection did not pick up a spike that would clearly indicate Detonation
Thanks in advance for any assistance/ guidance
-T
There are many aspects of the investigation I cannot talk about based on contracts/ legal constraints, so I posed the Question as general one about literature for my research/ investigation. I am currently digging through the AMS Hbk 12 on Fractography.
Background:
I'm a materials engineer with a fair bit of experience in failure analysis and fractography (abt 15 yrs)
The Ordnance was known and intended, a portion of the housing system failed in a closed-system.
I believe I have narrowed down the origin point of the housing failure as a whole (eliminating origin features on other debris items as secondary)
The event was so quick (1-2 ms) the pressure transducer data collection did not pick up a spike that would clearly indicate Detonation
Thanks in advance for any assistance/ guidance
-T