I originally posted this in the geotech forum but there very little traffic there!
I was looking for some suggestions to repair this segmental retaining wall that was not constructed correctly in the first place. After a section of the wall collapsed, I was called to inspect it and found out that there was no geo-grid installed and now, after over ten years, there are signs of movements but mostly at the top of the walls. Plan and photo are attached.
The blocks are not the interlocking type and can even slide on each other. There is a filter fabric directly behind the wall with about a couple of inches of crushed stone.
I was thinking of using soil anchors like Manta-Ray and build a CMU wall section by section as we remove and replace the existing blocks. This way, the CMU wall and the anchor will hold back the soil and the blocks could be used as decorative facing. I also thought about gravity walls but they are big and take too much space and not practical here.
The only info I have on soil is that this was cut into a hill and it’s about 500’ from ocean. There is no way I can get boring done at the top.
Any suggestion is appreciated.
I was looking for some suggestions to repair this segmental retaining wall that was not constructed correctly in the first place. After a section of the wall collapsed, I was called to inspect it and found out that there was no geo-grid installed and now, after over ten years, there are signs of movements but mostly at the top of the walls. Plan and photo are attached.
The blocks are not the interlocking type and can even slide on each other. There is a filter fabric directly behind the wall with about a couple of inches of crushed stone.
I was thinking of using soil anchors like Manta-Ray and build a CMU wall section by section as we remove and replace the existing blocks. This way, the CMU wall and the anchor will hold back the soil and the blocks could be used as decorative facing. I also thought about gravity walls but they are big and take too much space and not practical here.
The only info I have on soil is that this was cut into a hill and it’s about 500’ from ocean. There is no way I can get boring done at the top.
Any suggestion is appreciated.