Hello All ;
Have you ever seen a 4 - leg - yoke being used on magnetic particle test ?
If "yes" , is it acceptable and / or recognized by any Standard or Code ?
To my knowledge , the magnectic field created by a 4-leg - yoke is neither longitudinal , nor circular , and US does not make use of it.
Thank you.