API 650 clause 7.5.5.2.a. states where a concrete ring wall is provided under the shell, the top of ring wall shall be ........
API 650 clause 7.5.5.2.b. states where a concrete ring wall is not provided under the shell, the foundation under the shell shall be ...
If we have impregnated board on the concrete ring wall and the annular plate rest on this impregnated board, I should follow clause 7.5.5.2. b.
Your comments is highly appreciated.
Syah
API 650 clause 7.5.5.2.a. states where a concrete ring wall is provided under the shell, the top of ring wall shall be ........
API 650 clause 7.5.5.2.b. states where a concrete ring wall is not provided under the shell, the foundation under the shell shall be ...