T=1500F
P=80psia
Combustion Products
I dont have access to the B33.1 code and am currently doing preliminary work study feasibility of a rig that may be constructed in the future.
The Pipe will be a Nickel alloy, probably Hastelloy X and I have a great deal of material test information at elevated temperatures. I just want an idea of what FOS to use on a system like this. I was planning on using FOS=4. Just want to know your thoughts.
Any Help is greatly appreciated.