Hi All

I would like to know if it is possible to heat and form a polypropylene part. I have a half sphere and would like to have a flat surface on it. Can I apply heat to soften the material and form a flat surface? The thickness of the material is approximately 5/32". Do I have to be concerned with property changes? I.E. spidering, cracking and weakening of the material?


Tofflemire
 
Replies continue below

Recommended for you

Polypropylene is one of those wonderful materials known as a thermoplastic. You can heat it, melt it, and resolidify it without changing its chemical properties. You should be able to take a flat piece of metal, heat with with a blow torch and press it down on that ball to get the effect you're looking for. Polypropylene has a fairly low melting temperature, and it's not advisable to heat the whole part. You'll likely get deformation.

aspearin1
 
PP is a high shrinkage material, and while it can easily be thermoformed as described correctly above, it is prone to differential shrinkage and therefore warpage, so you will get a flatish surface, but truely flat will prove difficult if not impossible. It really depends on just how flat you want.

eng-tips, by professional engineers for professional engineers

Regards
pat

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor