stressguyMike
New member
Good morning,
I am working on a 6 ft. long extrusion m/f 6061-T6511. The part is thick, 0.125 in.
The part must be bent to a large radius. The max offset from horizontal is nearly 8 in.
Currently, the drawing has the part formed in the -T6511 condition. The drawing also has a note that says the formed part must be inspected for cracking and local buckling.
If I analyze the part as a 72 in. simply supported beam with max mid-span deflection equal to 8 in. I get a bending stress essentially equal to Ftu.
Therefore, I proposed to the designers the following options:
1. Procure in -T4511 condition, form, then heat treat to -T6511
2. Form in the W condition, age to -T42, then heat treat to -T62
3. Anneal the material, form in annealed condition, heat treat & age to -T62
So a number of questions:
1. Is this a legit issue?
2. If this is legit, what about all the formed parts out there, hat sections, channels, etc. that are formed. As long as min bend radii is met, no need to stress relieve.
Looking forward to some enlightenment!
Thank you,
Mike
I am working on a 6 ft. long extrusion m/f 6061-T6511. The part is thick, 0.125 in.
The part must be bent to a large radius. The max offset from horizontal is nearly 8 in.
Currently, the drawing has the part formed in the -T6511 condition. The drawing also has a note that says the formed part must be inspected for cracking and local buckling.
If I analyze the part as a 72 in. simply supported beam with max mid-span deflection equal to 8 in. I get a bending stress essentially equal to Ftu.
Therefore, I proposed to the designers the following options:
1. Procure in -T4511 condition, form, then heat treat to -T6511
2. Form in the W condition, age to -T42, then heat treat to -T62
3. Anneal the material, form in annealed condition, heat treat & age to -T62
So a number of questions:
1. Is this a legit issue?
2. If this is legit, what about all the formed parts out there, hat sections, channels, etc. that are formed. As long as min bend radii is met, no need to stress relieve.
Looking forward to some enlightenment!
Thank you,
Mike