Jul 12, 2013 #1 fedaqui Aerospace Joined Jul 12, 2013 Messages 2 Location US We would like to forge C93800 material. Could someone please provide a recommended forging temperature of C93800 bronze alloy? We plan on heating, pressing in a mechanical 2500 ton forge press, and then rolling to a certain diameter. Thanks David
We would like to forge C93800 material. Could someone please provide a recommended forging temperature of C93800 bronze alloy? We plan on heating, pressing in a mechanical 2500 ton forge press, and then rolling to a certain diameter. Thanks David
Jul 12, 2013 #2 jwhit Materials Joined Apr 3, 2012 Messages 202 Location US C93800 is one of the casting grades. You might look at the Copper Development Association website for information on an equivalent wrought grade. Upvote 0 Downvote
C93800 is one of the casting grades. You might look at the Copper Development Association website for information on an equivalent wrought grade.
Jul 12, 2013 1 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US David, Bronze with 2-4% Pb is considered the limit for acceptable forging. This alloy is not intended for hot working. Upvote 0 Downvote
David, Bronze with 2-4% Pb is considered the limit for acceptable forging. This alloy is not intended for hot working.