We would like to forge C93800 material. Could someone please provide a recommended forging temperature of C93800 bronze alloy? We plan on heating, pressing in a mechanical 2500 ton forge press, and then rolling to a certain diameter.

Thanks David
 
Replies continue below

Recommended for you

C93800 is one of the casting grades. You might look at the Copper Development Association website for information on an equivalent wrought grade.
 
David,

Bronze with 2-4% Pb is considered the limit for acceptable forging. This alloy is not intended for hot working.
 