Dear Colleagues, I need your opinion(s) one more time.

Recently I came across some new welds in stainless steel piping (built to ASME B31.3) with some degree of magnetism.

I have not used ferrite scope yet, but I will very soon. I've requested WPS/PQR to determine FN according to WRC-1992 FN diagram.

I know that ASME Section II, part C A6 pretty much describes what WRC established and from my previous life most refiners consider acceptable FN between 3 & 11.

Question 1) Does ASME B31.3 address ferrite content in weld deposits?

Question 2) If I find a FN > 11. What impact will have on corrosion properties and cryogenic properties?

Any links will be greatly appreciated.

Thanks,

Corgas

 
Replies continue below

Recommended for you

1)Not specifically, hence the coverage in API RP 582

2)The implications for in service performance are discussed in the SFA consumable specifications such as SFA-5.9, clause A.7. The corrosion performance will depend upon the environment to which the material is exposed.

Steve Jones
Materials & Corrosion Engineer
 
Please don't double post. Most of us are reading multiple forums.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thanks Steve.

Yes, SFA5.9 and SFA5.4 both describes same thing regarding ferrite.

1) is there a graph where it shows % ferrite Vs. toughness for austenitic SS?

1) What's the correlation between % ferrite Vs. Corrosion resistance (Ex: PREN) for austenitic SS?

Corgas
 