metengr. Thanks for the input. I am doing much of what you mention. We use 625 overlay on the boiler furnace walls for wastage. We shield tubes with SS shields and in some areas have to reshield them again in 6 months.
You are right that ducts are a minor issue until the leakage because so much that the plant is derated due to ID fan amps. We were limited 50 MW limping into last outage due to duct leaks.
As for the problem looking worst than it really is...When you have holes in your turning vanes big enough to drive a school bus thru then there is no need to UT check the thickness!
I have experimented with weld overlay, AR plate, Chome carbide cladding, Tungsten Carbide clading, ceramics, Gunnite, Envelope shields, white iron, vanadium alloys, denzit, trowlable ceramic, conforma clad etc. I don't think we are anywhere near finding the optimum solution. Some work good but are outrageously expensive, some are cheap and don't work.
My question to the community is are there optimum solutions and lots of bang for the buck that have been found in similar abrasive type applications.