I was trying to find somewhere in ASME B31.3 Process Piping Code that would cover a flush patch insert (full penetration groove weld)on piping.
One of our clients has requested we remove an existing o-let (where the attachment weld has failed) on a line and replace it with a flush patch cut from the same diameter pipe. The Code of Construction is B31.3 "Normal Fluid Service". This a hydrocarbon system and operates around 200 PSI. The flush patch will be examined 100% by the RT method.
My concern is that B31.3 does not cover this type repair, as opposed to just maybe welding in a new joint. We have written authorization to proceed but I'm still a little concerned with liability and also prefer to know for myself.
Please Advise!
One of our clients has requested we remove an existing o-let (where the attachment weld has failed) on a line and replace it with a flush patch cut from the same diameter pipe. The Code of Construction is B31.3 "Normal Fluid Service". This a hydrocarbon system and operates around 200 PSI. The flush patch will be examined 100% by the RT method.
My concern is that B31.3 does not cover this type repair, as opposed to just maybe welding in a new joint. We have written authorization to proceed but I'm still a little concerned with liability and also prefer to know for myself.
Please Advise!