We have a 7.5" I.D. FPSO Flexible riser from which we have recovered, topside, sections of the internal SS carcass and pressure retaining sheath.
The riser is 300m long, with a mid arch bouy, water depth 90m in production service for 4 years.
We are looking to perform an internal camera investigation to determine the location / extent of the fault with the purppose of determining repair potential.
We are really hoping to find a company with a track record. We have plenty of "we've got a camera but never done it before" possibles.
Anybody had any success with a venture like this??

Thanks

Roy
 