Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Flex Fatigue of PFA Tubing - Relating MIT Tester Results to Reality

Status
Not open for further replies.

wdornfeld

Mechanical
Joined
Mar 26, 2001
Messages
16
Location
NL
I have an application where one end of a ~12" length of 8x6mm Perfluoralkoxy PFA ultra high purity tubing is continuously cycled about 3/4" sideways (+/- 3/8"). I can find "MIT Flexural Life" (ASTM D2176) properties of PFA that report 200,000 cycles of life. I believe that the MIT tester is flexing samples that are between 10 and 30 mils thick around a 15 mil radius nose. I calculate this as putting between 25 and 50% alternating strain on the material, respectively - pretty darned big. I am used to S-N diagrams for ductile metals, and am looking for how to relate my application strain to the MIT tester results to estimate life for my case. Thanks for any guidance.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top