Hello,
I currently work for a company that makes products out of moly alloys, aluminum and stainless steel. These products are about 1 mm to 4 mm thick and 100mm to 300 mm in width. These products are sent out to be anodized or coated for some sort of protection.
When the parts are sent back we check to correct the flatness of the pieces, which are usually out of spec. The flatness is corrected by bending the parts over angle iron, marble slabs, and rods, all surfaces are protected to prevent scratches to the coated surface.
Our inspection team has become quite proficient at correcting flat parts on these pieces. However the learning curve is quite high and the work can be very tedious on high volume orders. Throwing more people to straighten the pieces results in little improvement since all are not trained or experienced.
I was wondering if anyone had any processes or methodologies, outside of bending the pieces by hand, that would streamline the correction process.
Thank you
_Brian
I currently work for a company that makes products out of moly alloys, aluminum and stainless steel. These products are about 1 mm to 4 mm thick and 100mm to 300 mm in width. These products are sent out to be anodized or coated for some sort of protection.
When the parts are sent back we check to correct the flatness of the pieces, which are usually out of spec. The flatness is corrected by bending the parts over angle iron, marble slabs, and rods, all surfaces are protected to prevent scratches to the coated surface.
Our inspection team has become quite proficient at correcting flat parts on these pieces. However the learning curve is quite high and the work can be very tedious on high volume orders. Throwing more people to straighten the pieces results in little improvement since all are not trained or experienced.
I was wondering if anyone had any processes or methodologies, outside of bending the pieces by hand, that would streamline the correction process.
Thank you
_Brian