Not that I cannot weld the full depth of the groove for a Flare-Bevel weld, but assuming I did not want to, how do you calculate the effective throat? I have not found any actual examples.
In my case, I have a 5/8" diameter round rod to be welded to a flat plate. If I only wanted to go up 1/4" from the center of the rod and not the 5/16", what would I look at to calculate the effective weld? What 2 points do I measure from?
I know the full depth weld would be (5/16)*R = .0977.
In my case, I have a 5/8" diameter round rod to be welded to a flat plate. If I only wanted to go up 1/4" from the center of the rod and not the 5/16", what would I look at to calculate the effective weld? What 2 points do I measure from?
I know the full depth weld would be (5/16)*R = .0977.