Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Flare Bevel Groove Weld Effective Size

Status
Not open for further replies.

LowLax

Structural
Joined
Feb 22, 2005
Messages
93
Location
US
Why (according to AISC 13th ed) is the effective size of a flare groove weld 5/16R with SMAW and 5/8R with GMAW?

Seems like a big difference. There's obviously something I don't understand about the difference in welding processes.
 
It may be due to the higher currents used with the GMAW using spray mode transfer. The higher current typically results in greater joint penetration.

I tend to be conservative and stay with the limitations provided by AWS D1.1.

If you have any concerns with the increased weld size permitted by AISC, make a couple of samples that replicate the joint detail you are considering (the diameter of the round is important). If the macroetches of the samples suport the increased weld size as permitted by AISC, make sure your welders are using the same welding parameters as those used used to weld the samples.



Best regards - Al
 