Fine Grained SA 106 GrB/SA 105

Status
Not open for further replies.

Peter113

Materials
Oct 17, 2007
19
Hi,
for a normalized SA 106 GrB and SA 105, is it supposed to be a fine grained material as well?
Thanks
Peter
 
Replies continue below

Recommended for you

Peter113;
No. Normalized results in a more uniform grain size, not necessarily fine grain. This is a specified practice.
 