Kannn

Mechanical
Jul 5, 2021
8
Hello engineers , i have a leak from a fin fan cooler , its type is plug type fin fan air cooler , the leak is from the strength weld between the tube and the tube sheet ( the strength weld had failed ) , i want to elimnate the leak , i know that plug will not be that sufficient, is there any way that i can repair this , like an expander to enter inside the water box and expand the tube , attached images for illustration



Waiting your support and help
Thanks

 
Replies continue below

Recommended for you

Ream the tube ends and remove it.
Then weld plugs into the holes in tubesheet.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 