Hello All,
I have few questions regarding Fillet Weld Procedure Qualification.
Per Figure QW-462.4(d), the Max. fillet size shall be equal to T - which is the Pipe wall thickness.
1. Does the "Max. fillet size" refer to the weld leg or throat?
2. In order to qualify the procedure, are the only requirement to be meet are those shown in QW-183?
3. In case that the actual fillet size (in the actual welded test coupon) is larger than T, does a new Test Coupon and Certification of the welding procedure is needed?
Thanks,
I have few questions regarding Fillet Weld Procedure Qualification.
Per Figure QW-462.4(d), the Max. fillet size shall be equal to T - which is the Pipe wall thickness.
1. Does the "Max. fillet size" refer to the weld leg or throat?
2. In order to qualify the procedure, are the only requirement to be meet are those shown in QW-183?
3. In case that the actual fillet size (in the actual welded test coupon) is larger than T, does a new Test Coupon and Certification of the welding procedure is needed?
Thanks,