Duwe6,
Your interpretation is correct based on ASME / AWS terminology but it differs in other countries.
Lack of penetration or incomplete penetration is the terminology used for fillet welds in Australia, New Zealand, Britain and Europe.
If there are unfused areas (straight lines)between weld metal and parent metal on the vertical or horizontal plate it is called Lack of Fusion.
If the weld metal does not envelop the junction of the vertical and horizontal plates it is called Lack of Penetration or Incomplete Penetration.
It seems even some Americans use similar terminology
Analysis Of A Fractured Crane Frame Weldment
Report for: Report by:
**************
**************
**************
**************
************** METALLURGICAL TECHNOLOGIES, INC., P.A.
160 Bevan Drive
Mooresville, NC 28115
704-663-5108
SUMMARY:
A fractured pipe/flange weldment from a crane frame assembly was received for analysis to determine the cause of fracturing along the circumferential fillet weld. Results indicate the fracture occurred by cyclic fatigue crack growth that initiated at the root of the fillet weld due to incomplete penetration by the root pass and a lack of fusion to the pipe or flange at several locations around the weldment.
Microscopic and metallographic examination revealed fatigue crack initiation sites at and between the incomplete penetration and lack of fusion sites. The lack of penetration was noted around 60% of the circumferential fillet weld. Lack of fusion to the pipe and flange were noted around approximately 50% of the weld.
The flange and pipe were manufactured from weldable grades of high strength, low alloy structural steels. A compatible low alloy steel filler metal was used. Hardness testing across the weldment revealed no unusual softening or embrittlement.
Regards,
Kiwi