If PQR refer to AWS A5.1 E6011/E7016, but WPS refer to AWS A5.1 E6013. Is this acceptable in ASME IX?
 
Replies continue below

Recommended for you

If PQR refer to AWS A5.1 E6011/E7016, but WPS refer to AWS A5.1 E6013. Is this acceptable in ASME IX?

Reply; No, the essential variables for procedure qualification using the SMAW process are a change in F-No and A-No for electrodes.

SFA 5.1 EXX11 is F-No 3
EXX13 is F-No 2
 