Fiber angles are probably held to no more than +/-0.25° in the barrel section and +/-2° in the end domes. Ply thickness will be a function of how tight the resin content is held on the prepreg or wet winding process. The tolerance on cured ply thickness of prepreg materials (nominal thickness ~ 0.008 unch) is typically not less than +/-0.0001 inch (+/-0.0025 mm)