Hi everyone,
I designed a slab for a mine closure application.
To prevent workers from working above an open raise, Slabs are to be poured on the ground, then lifted and placed on a fill raise.
The operations proposed a modification. The idea is to install styrofoam prior to pour. Upon cure, we will push forks through foam for manipulating the slabs.
The issue is long term stability here. I know crack will form eventually and reach the steel.
Any thoughts on the issue.
I also Added a sketch. See attached pdf.
Charles, mine engineer
Ingenieur Minier. QuTbec, Canada.