Hi,
I had a list of materials sent to me today with the question are the materials ferromagnetic or not?
- ASTM A193 B7M,
- 18-8 st steel,
- BS 1449 HR4,
- ASTM A216 WCB,
What I have found out so far is that 18-8 stainless (ally 304) is austenitic and not ferromagnetic. ASTM A193 B/M is listed in the standard under ferritic material, and hence should be ferromagnetic. As far as I can find BS 1449 HR4 and ASTM A216 WBC are both ferromagnetic. Can anyone please confirm if my findings are correct or give input to the correct answer.
Thank you
I had a list of materials sent to me today with the question are the materials ferromagnetic or not?
- ASTM A193 B7M,
- 18-8 st steel,
- BS 1449 HR4,
- ASTM A216 WCB,
What I have found out so far is that 18-8 stainless (ally 304) is austenitic and not ferromagnetic. ASTM A193 B/M is listed in the standard under ferritic material, and hence should be ferromagnetic. As far as I can find BS 1449 HR4 and ASTM A216 WBC are both ferromagnetic. Can anyone please confirm if my findings are correct or give input to the correct answer.
Thank you