I have a couple of questions about FCAW and SAW Welding process.
(1) The vessel (SA516-70N) MDMT is -50F.
Can I use F7XT-9 as the filler metal and do impact test for the weld at -50F on the PQR? I am worried about it because it is recommended to do impact test at -40F (ASME II PARTC SFA5.20). Does it means that this filler metal can not be used at a temperature lower than -40F?
(2)The vessel (SA516-70, No PWHT) MDMT is -20F.
Can I use Flux F7A4 and do impact test for the weld at -20F on PQR?
(3)The vessel (SA516-70N, No PWHT) MDMT is -50F.
Can I use Flux F7A4 and do impact test for the weld at -50F on PQR?
Thanks.
(1) The vessel (SA516-70N) MDMT is -50F.
Can I use F7XT-9 as the filler metal and do impact test for the weld at -50F on the PQR? I am worried about it because it is recommended to do impact test at -40F (ASME II PARTC SFA5.20). Does it means that this filler metal can not be used at a temperature lower than -40F?
(2)The vessel (SA516-70, No PWHT) MDMT is -20F.
Can I use Flux F7A4 and do impact test for the weld at -20F on PQR?
(3)The vessel (SA516-70N, No PWHT) MDMT is -50F.
Can I use Flux F7A4 and do impact test for the weld at -50F on PQR?