This material is highly corrosion resistant, which is why I am posting this question here.

I am looking for fatigue properties for Nitronic 50, particularly as they relate to Endurance Limit, Fatigue Strength, Number of cycles N versus Strength Sa. Specifically, we care about very high cycle fatigue, where N is greater than 1e8 cycle life.

Thanks for any help.
 
Replies continue below

Recommended for you

For which condition, as cold worked to higher strength or the annealed condition?
The only data that I have is for cold worked material.

A quick internet search comes up with:
Rotating beam fatigue, 10e8 cycles for 1" bar
annealed 47ksi (this should be 55-60ksi yield, 110-120ksi UTS)
HS (as hot rolled) 68ksi

This stuff has been used for prop shafts in boats for decades so there should be a lot of fatigue data out there.


= = = = = = = = = = = = = = = = = = = =