I am looking for fatigue curves of unnotched A6Z1.
In "Smithells Light Metals Handbook" I have found some data for R=-1. I have found also on MIL-HDBK-5H some curves for AZ31B-F (figure 4.2.1.4.8 (a)). It is stated that "AZ61A is much like AZ31B in general characteristics" but if I compare data from this two references, some discrepancy exisits (for 10e7 cycles, 69MPa is given in MIL-HDBK-5H while 124MPa in the Smithells...)
Someone has some data for this kind of material?
Thank you in advance
I am looking for fatigue curves of unnotched A6Z1.
In "Smithells Light Metals Handbook" I have found some data for R=-1. I have found also on MIL-HDBK-5H some curves for AZ31B-F (figure 4.2.1.4.8 (a)). It is stated that "AZ61A is much like AZ31B in general characteristics" but if I compare data from this two references, some discrepancy exisits (for 10e7 cycles, 69MPa is given in MIL-HDBK-5H while 124MPa in the Smithells...)