Nov 7, 2005 #1 keebs Mechanical Joined Jul 29, 2003 Messages 14 Location US Does anyone know of published fatigue curves for metric socket head cap screws? Thanks keebs
Nov 7, 2005 #2 boo1 Mechanical Joined Oct 31, 2001 Messages 2,129 Location US The fatigue curve is a function of the material. Stress concentrations offset the curve. Upvote 0 Downvote
Nov 8, 2005 3 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US keebs, Unbrako/SPS has publisehed data on fatigue strength of their SHCS. Their Engineering Guide is available using the following link: http://www.unbrako.com/Engineer_guide.htm Upvote 0 Downvote
keebs, Unbrako/SPS has publisehed data on fatigue strength of their SHCS. Their Engineering Guide is available using the following link: http://www.unbrako.com/Engineer_guide.htm
Nov 8, 2005 Thread starter #4 keebs Mechanical Joined Jul 29, 2003 Messages 14 Location US Thanks TVP for the link. Upvote 0 Downvote
Nov 8, 2005 #5 Pwalk Mechanical Joined Apr 27, 2005 Messages 2 Location GB Hi You could try BS 7608, not specific to cap screw but gives S-N data for various steel joints. Upvote 0 Downvote