Does anyone know of published fatigue curves for metric socket head cap screws?

Thanks
keebs
 
The fatigue curve is a function of the material. Stress concentrations offset the curve.
 
Thanks TVP for the link.
 
Hi

You could try BS 7608, not specific to cap screw but gives S-N data for various steel joints.
 