alansimpson
Mechanical
I am doing R&D work on magnets and I wish to bond Ni plated magnets to polycarbonate in many different configurations. I need a fast adhesive so that I can place and bond many different configurations in a reasonable amount of time. 10-20 sec. per magnet. Currently I am using cyanoacrylate. This has poor bonding to magnet and poor gap filling when shapes get complicated. I also tried an acrylic with primer which was too slow. A UV set adhesive sounds good except for the expense of the lamp.
Know of any adhesives out there?
Thanks.
Know of any adhesives out there?
Thanks.