The 28 day compressive strength for S type mortar came near 700 PSI. This is well short of the 1700 psi specified strength. The walls do not have much vertical loads on them. However, they are shear walls. WE have cubes that will be tested at 56 days. I do not think they will come any were near specified strength based on the 7 and 28 day breaks. I have two questions as follows:
1.What options available to remedy this situation. (I am thinking of asking the contractor to fill all cells solid with grout as one option).
2.Will taking prisms from the wall for testing add any value?
Regards,
Lutfi
1.What options available to remedy this situation. (I am thinking of asking the contractor to fill all cells solid with grout as one option).
2.Will taking prisms from the wall for testing add any value?
Regards,
Lutfi