mkolwankar
Mechanical
I have following metallurgy combinations for S&T Heat Exchangers. I would like to know any fabrication limitations with the below metallurgy for tubes & tubesheets.
For one exchanger
Tube Material - 13 Cr
Tube sheet material - CS + 13Cr cladding on both sides
Tube - Tube sheet joint - Expanded in two groves
For other exchanger
Tube Material - 13 Cr
Tube sheet material - CS + 13Cr cladding on tube side
Tube - Tube sheet joint - Expanded
Thank you.
For one exchanger
Tube Material - 13 Cr
Tube sheet material - CS + 13Cr cladding on both sides
Tube - Tube sheet joint - Expanded in two groves
For other exchanger
Tube Material - 13 Cr
Tube sheet material - CS + 13Cr cladding on tube side
Tube - Tube sheet joint - Expanded
Thank you.