Here is my understanding of D1.1-2020, Clause 5 and 6.2
Steel Fab Shop A has a single owner and 20 employees
All the employees leave to start Fab Shop B.
Fab Shop B cannot bring with them any of the WPS or PQR documents, but instead must start from scratch - PQR and WPS.
Fab Shop A hires a new bunch with lower skill and no knowledge of the PQRs, but the WPS records stay with the original company regardless of the wholesale personnel change. Shop A new staff takes ownership of existing PQRs and WPS in the binder, even if they have no idea how to write one themselves.
Correct?
I realize similar questions have been asked previous on this post - looking for an Amen or blunt correct.
Steel Fab Shop A has a single owner and 20 employees
All the employees leave to start Fab Shop B.
Fab Shop B cannot bring with them any of the WPS or PQR documents, but instead must start from scratch - PQR and WPS.
Fab Shop A hires a new bunch with lower skill and no knowledge of the PQRs, but the WPS records stay with the original company regardless of the wholesale personnel change. Shop A new staff takes ownership of existing PQRs and WPS in the binder, even if they have no idea how to write one themselves.
Correct?
I realize similar questions have been asked previous on this post - looking for an Amen or blunt correct.