Good morning, I have a regular steel beam HSS20x12x5/8(Fy46ksi) that was specified to be weld with fillet weld with electrode EXX70, but the contractor use an electrode E306L-16.
Is there any restriction to use this electrode in lieu of the EXX70.
 
I would like to see the WPS that says to weld it with 309.
 
309???

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Reject it; even if he has a qualified welding procedure.
 
for what reason, other than procedural? Best to find out if it works?

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Greater residual welding stress due to dissimilar metals shrinkage.
 