Feb 2, 2024 #1 Mario M. Structural Joined Feb 2, 2024 Messages 1 Location US Good morning, I have a regular steel beam HSS20x12x5/8(Fy46ksi) that was specified to be weld with fillet weld with electrode EXX70, but the contractor use an electrode E306L-16. Is there any restriction to use this electrode in lieu of the EXX70.
Good morning, I have a regular steel beam HSS20x12x5/8(Fy46ksi) that was specified to be weld with fillet weld with electrode EXX70, but the contractor use an electrode E306L-16. Is there any restriction to use this electrode in lieu of the EXX70.
Feb 2, 2024 #2 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA I would like to see the WPS that says to weld it with 309. Upvote 0 Downvote
Feb 2, 2024 #3 dik Structural Joined Apr 13, 2001 Messages 26,126 Location CA 309??? -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik Upvote 0 Downvote
309??? -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik
Feb 5, 2024 #4 weldstan Materials Joined Jun 24, 2011 Messages 2,808 Location US Reject it; even if he has a qualified welding procedure. Upvote 0 Downvote
Feb 5, 2024 #5 dik Structural Joined Apr 13, 2001 Messages 26,126 Location CA for what reason, other than procedural? Best to find out if it works? -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik Upvote 0 Downvote
for what reason, other than procedural? Best to find out if it works? -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik
Feb 6, 2024 #6 weldstan Materials Joined Jun 24, 2011 Messages 2,808 Location US Greater residual welding stress due to dissimilar metals shrinkage. Upvote 0 Downvote