some aluminium supplier, for using DC-cast billets in forging industry,use from an preliminary extrusion operation.Why?
 
The preliminary extrusion operation refines the grain size (makes it smaller) and removes many of the other defects inherent in cast structures (variable grain size & orientation, porosity, etc.). Smaller, more homogeneous grains result in higher formability and reduced cracking during forming.
 
Dear TVP,
COULD YOU PLEASE,GIVE ME SOME INFORMATION,REGARDING TO AS-FORGED & AS-EXTRUDED PROPERTIES OF 6082 WROUGHT AL ALLOYS,AS WELL AS ABOUT ITS MICROSTRUCTURE ?THANKS IN ADV.
 