Hello!
For a casting using investment casting process in CF3 (SS 304) material, There is extra metal dots coming in letters of company symbol of customer.
For example, If letter is 'B' then holes of extruded 'B' on castings gets filled with extra metal. I have tried to avoid this extra metal by doing some experiments like decreasing extrude height of letters from 0.5mm to 0.3mm but there are no successful results acheived.
It would be great, If anyone can help me to avoid this thing by suggesting any remedies for that.
for info. only: This may occur in shelling process of wax patterns as it can not fill whole cavity of extruded letters on wax pattern.
aiming towards industry 4.0
For a casting using investment casting process in CF3 (SS 304) material, There is extra metal dots coming in letters of company symbol of customer.
For example, If letter is 'B' then holes of extruded 'B' on castings gets filled with extra metal. I have tried to avoid this extra metal by doing some experiments like decreasing extrude height of letters from 0.5mm to 0.3mm but there are no successful results acheived.
It would be great, If anyone can help me to avoid this thing by suggesting any remedies for that.
for info. only: This may occur in shelling process of wax patterns as it can not fill whole cavity of extruded letters on wax pattern.