Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

External Paint System for Vessels that are to be Steam Cleaned

Status
Not open for further replies.

balven

Materials
Aug 29, 2011
9
Dear all,

This post is regarding the type of external painting system that should be specified on carbon steel vessels to be cleaned with steam (at atmospheric pressure). The steam temperature is close to 180 deg. C. Does the steam out condition need to be considered while specifying the external paint system ? If a vessel’s max. operating temperature is, say 30 deg. C but it has to be steam cleaned, can I specify the 3-coat external paint system (zinc-rich epoxy primer + high build epoxy intermediate coat + polyurethane topcoat) ? What is the risk involved and how can it be mitigated ?

Request you to kindly share your experience in this matter.

Regards,
Balvendra Pal
 
Replies continue below

Recommended for you

How long and how much is this ( I assume internal) steam cleaning expected to last for (max) and what is the dimensions of the pressure vessel?
 
Hi Cloa, the steam cleaning is internal, and is expected to last for 3-4 hours. There are several such pressure vessels of various sizes.
 
What is the smallest vessel? At what rate is steam max output?
 
So, would that maximum operating temperature not need resetting? Get some heat transfer calculations done to assess the temperature that will be achieved at the steel coating interface, and then confirm with the paint manufacturer that this temperature is tolerable for intermittent short term exposure.

Steve Jones
Materials & Corrosion Engineer


All answers are personal opinions only and are in no way connected with any employer.
 
If you use IOZ/Epoxy/PUR you should be alright. IOZ will handle heat up to 400 C
 