rmillercwi
Materials
We are building several carbon steel tube panels (upper/lower header joined with boiler tubes) and the client is asking for final hardness testing. Nothing special about the project. ASME Sect I. Header pipe SA 106C, sa 51670 end plates and SA 192 finned tubes. PWHT per pw.39 for P1 materials
I have never had this come up before. Having some trouble finding what the final harndness number should be max/min. Thinking 200 BHN max is appropriate? E70T1 flux core/100% co2 on nozzles and er70s-2 GTAW on tube to header welds.
I have never had this come up before. Having some trouble finding what the final harndness number should be max/min. Thinking 200 BHN max is appropriate? E70T1 flux core/100% co2 on nozzles and er70s-2 GTAW on tube to header welds.