We are in the process of fabricating heat exchanger where the shell side is to be tested at 770PSIG. The tube sheet has 2 grooves and the tubes will be welded with 2 passes.
My question is as follows.
1) should expansion be performed before or after welding
2) Is Hydraulic expansion a better option than coventional roller expansion.
3) Is helium test required prior to Hydrostatic test to ensure no leakage .
Thanks
My question is as follows.
1) should expansion be performed before or after welding
2) Is Hydraulic expansion a better option than coventional roller expansion.
3) Is helium test required prior to Hydrostatic test to ensure no leakage .
Thanks