Galway11
Civil/Environmental
- Mar 29, 2011
- 8
Hello everyone,
I need to seal 20mm x 20mm expansion joints with hot applied modified bitumen sealant. This is for a lightly trafficked outdoor concrete hardstanding.
The problem is the filler is closed cell polyethlyene foam (as specified by designers), which I'm told will be melted by hot applied sealant. Cold pour is not an option due to cost...
The best solution I can find is to use 3m 7130 masking tape as a bond breaker (heat resistant to 170 degrees C supposedly). But I haven't done this before so I don't know if it will work or not!!!
Anybody done this before? Is it likely to work?
Thanks in advance for any replies...
I need to seal 20mm x 20mm expansion joints with hot applied modified bitumen sealant. This is for a lightly trafficked outdoor concrete hardstanding.
The problem is the filler is closed cell polyethlyene foam (as specified by designers), which I'm told will be melted by hot applied sealant. Cold pour is not an option due to cost...
The best solution I can find is to use 3m 7130 masking tape as a bond breaker (heat resistant to 170 degrees C supposedly). But I haven't done this before so I don't know if it will work or not!!!
Anybody done this before? Is it likely to work?
Thanks in advance for any replies...