I am trying to track down a load table for a hollow core slab. Existing drawings (dated in 1984) call out: 6” core slab 57 type. Does anyone have any experience tracking down load tables for existing hollow core slabs?

Thanks in advance.

D2005500-1AE0-4B03-997A-A429093BD878_pkhv08.jpg
 
Replies continue below

Recommended for you

Hopefully someone else can produce the load tables but my guess would be five, seven wire strands per plank unit.
 