Hi everybody,
Have an Ermaksan fiber 2 kw since december last year. Went good for a month. Since that time they came 7 times trying to fix problems. Still problem and an another guy come over again this month. Well I think I found something.
I cut almost ss all the time. Since two weeks I change the power and it work much better like that. Still have dross but at the minimum. Easier working the piece after. They told me never change the power, but the piece were awful hot. It start the first 12 inches nice and slowly the dross appears bigger and bigger. If I keep going the program I'll success to cut everything but the big dross will be there. That is if I keep the power at 2000 watt. Like I said before, now I cut everything at 1900 with minimum dross and I have to push gaz at 19 bar for almost every tickness.
I have an excess heating. The first head they changed the miror was crack. I thought it was back reflexion but now I'm wondering if it was the heat from the laser. It's like the laser send me way too much power for what it suppose.
Does somebody already had a problem like that? What can be defective before the head?
ps thanks Macgiver for the lens clue. realy appreciate.Been in holyday for 3 weeks that,s why didn't answer
Have an Ermaksan fiber 2 kw since december last year. Went good for a month. Since that time they came 7 times trying to fix problems. Still problem and an another guy come over again this month. Well I think I found something.
I cut almost ss all the time. Since two weeks I change the power and it work much better like that. Still have dross but at the minimum. Easier working the piece after. They told me never change the power, but the piece were awful hot. It start the first 12 inches nice and slowly the dross appears bigger and bigger. If I keep going the program I'll success to cut everything but the big dross will be there. That is if I keep the power at 2000 watt. Like I said before, now I cut everything at 1900 with minimum dross and I have to push gaz at 19 bar for almost every tickness.
I have an excess heating. The first head they changed the miror was crack. I thought it was back reflexion but now I'm wondering if it was the heat from the laser. It's like the laser send me way too much power for what it suppose.
Does somebody already had a problem like that? What can be defective before the head?
ps thanks Macgiver for the lens clue. realy appreciate.Been in holyday for 3 weeks that,s why didn't answer