Has anyone seen, or does anyone have, a video showing spark test results useful to identify carbon steel, cast iron, nodular iron, low alloy steel, etc?
Even if the test needs to be done in a dark room or under some specified conditions, perhaps with a particular grinding wheel.
Maybe superb color photos would work.
The immediate intent is to ID materials for weld repairs. Cast steel, cast iron, ductile/nodular iron.
thanks,
Dan T
Even if the test needs to be done in a dark room or under some specified conditions, perhaps with a particular grinding wheel.
Maybe superb color photos would work.
The immediate intent is to ID materials for weld repairs. Cast steel, cast iron, ductile/nodular iron.