1. Without more details, this is not an easy question. Electroetching with 10 % oxalic acid, Kalling's, Beraha's, Ralph's, and others are all possibilities.
2. Weld metal/fusion zone should be distinct from HAZ after etching.
3. Different mechanisms are present for different etchants. Anodic dissolution of grain boundaries, sulfide film formation, and others are present.