Dear All,
I have 2 materials. One with normalized and other Normalized and tempered.
I have qualified a PQR -1 as per ASME SEC IX with impact requirements as per ASME B31.3 with base material normalized .
My job is having impact requirementsas per ASME B31.3 with normalized and tempered base material.
All the variables remains similar except heat treatment.
Can i use the PQR-1 for writing WPS to weld normalized and tempered base material?